239 RAKU CLAY - Cone 04-10 (Photo C/04)

239 RAKU CLAY - Cone 04-10 (Photo C/04)

An open clay body specially formulated to withstand the thermal shock of Raku firing. Contains sand. Suggested bisque temperature C/04. Shrinkage: 8% at C/04, 13% at C/6. Absorption: 17% at C/04, 4.5% at C/6.

239 RAKU CLAY - Cone 04-10 (Photo C/6)

239 RAKU CLAY - Cone 04-10 (Photo C/6)

An open clay body specially formulated to withstand the thermal shock of Raku firing. Contains sand. Suggested bisque temperature C/04. Shrinkage: 8% at C/04, 13% at C/6. Absorption: 17% at C/04, 4.5% at C/6.

295 RAKU CLAY WITH KYANITE - Cone 04-10 (Photo C/04)

295 RAKU CLAY WITH KYANITE - Cone 04-10 (Photo C/04)

Good for larger pieces. The addition of kyanite increases the strength of this body. Suggested bisque temperature C/04. Shrinkage: 5% at C/06. Absorption: 7.4% at C/06.